Description
AASHTO PP 100-20 for ultrathin bonded wearing course includes a mix design evaluation for the asphalt surface mixture, usually 1/2 to 1 in. (12.5 to 25.4 mm) thick, to determine the proportions of polymer-modified emulsified asphalt that is used as the tack coat, PG binder, mineral aggregate, mineral filler, and additives to produce an ultrathin bonded wearing course job-mix formula.
Product Details
- Published:
- 2020
- Number of Pages:
- 5
- File Size:
- 1 file , 900 KB
- Product Code(s):
- PP100-20-UL, PP100-20-UL, PP100-20-UL